CARIELLO, Mauricio Pompeu et al. Implant-supported titanium framework: photoelastic analysis before and after spark erosion procedure. Braz. J. Oral Sci. [online]. 2010, vol.9, n.1, pp. 48-53. ISSN 1677-3225.

AIM: This study used a photoelastic analysis to evaluate the passive fit of titanium cast laser welding frameworks before and after spark erosion procedure. METHODS: A stainless steel cast was used in order to reproduce a human mandible. Five Multi-Unit abutment analogs were attached to this cast and 6 frameworks were produced in commercial pure titanium. The cast was molded and a photoelastic matrix was produced incorporating 5 dental implants with Multi-Unit abutments. All samples were subjected to a laser welding. The precision of adjustments within a range of 0.5 μm was evaluated under microscope observation. The best fitted framework was selected and subjected to a photoelastic analysis (Group I). The tightening of the screws was in 3 predetermined sequences (1,2,3,4,5/ 5,4,3,2,1/ 3,2,4,1,5). Then the same framework was subjected to a refinement by spark erosion technique (Group II) and evaluated by photoelastic analysis. RESULTS: The sequence (3,2,4,1,5) achieved better results in both groups. A larger number of fringes were observed around the median implants in all sequences in both groups. CONCLUSIONS: The titanium cast laser welded frameworks processes associated with spark erosion procedure improves significantly the marginal framework adaptation and is effective for its passive fit.

Palavras-chave : titanium; misfit; implant; framework.

        · texto em Inglês     · pdf em Inglês